The same leather grain etched to 20 microns and to 40 microns gives two different finishes: the first is fine and slightly glossy, the second coarse, matte and draggy. With chemical-etched texture, the texture number defines only the shape of the pattern. What actually sets the feel and the gloss is the etch depth. Our order of selection is: fix the pattern family by application, then use depth to tune gloss, and finally add draft angle. Reverse that order and the first sampling run will be reworked.

Textures fall into three families, chosen by purpose before feel is discussed. Leather grain is irregular, with the longest streaks beyond 100 microns; its strength is hiding sink marks and flow lines, so large housings and parts with sink over ribs use it.梨地, or even round dots, feels fine and is distributed regularly, suited to parts held for a long time such as handles and knobs. Sandblast is a fine matte texture with the lowest gloss and the least fingerprint visibility, suited to frequently touched panels. Choosing the wrong one is not an aesthetic mistake but a functional one: a sandblasted handle feels draggy, while a coarse leather panel shows fingerprints and shine.

Depth decides gloss. Etching bites pits into the tool steel and the melt flows into them, so a deeper pit means a rougher face and lower gloss. A 20-micron leather grain reads about 60 to 70 GU at 60 degrees, close to semi-matte; at 40 microns it falls to 20 to 30 GU, a clearly coarse matte. As a working line, every extra 10 microns drops gloss by roughly 15 to 20 GU. The change in feel is even more direct: 20 microns feels fine and slightly slippery, 40 microns shows obvious grain resistance. Write a depth range on the CMF sheet, such as leather grain type S, 30 to 35 microns, so the first and later batches do not land in different bands.

The overlooked cost is draft angle. The grain lives as pits in the tool surface, and the plastic part must be pulled out of them; deeper grain means more resistance. A glossy face needs only 0.5 to 1 degree, but leather grain above 30 microns usually needs 1.5 to 3 degrees, and 40 microns needs 2 to 3. The working value is 0.5 to 1 degree of extra draft per 10 microns, less for rounded dots and more for sharp leather grain. Insufficient draft scores the grain or whitens and cracks the part, so the compensation must reach the structure engineer before drawings are issued, written into the 3D model, not left as a verbal note. At sampling, insist on samples in the same material and colour and sign off gloss and feel together; a texture card alone proves nothing.